Product Support Information
Support
To use ALPASTE® more effectively
Handling Instructions
Recommended Transportation and Handling Methods
- Avoid excessive shock, vibration, dropping, falling, or tipping over.
- To maintain quality (dispersibility), a slight excess of organic solvent is added, which may seep to the surface and change the state of the product inside the container (biphasic separation).
- If the container is damaged, there is a risk of organic solvent evaporation or the ingress of rainwater or foreign matter, which may lead to a decrease in dispersibility.
Recommended Storage Methods
- Store indoors away from direct sunlight and heat sources.
Low temperature: Precipitation of fatty acids
High temperature: May cause a decrease in dispersibility or swelling of the can due to solvent expansion. - Seal the product immediately after opening.
Evaporation of the organic solvent and absorption of moisture can lead to a decrease in dispersibility and may also cause contamination by foreign matter.
Potential Product Conditions
Regarding two-layer separation
Two-layer separation refers to a state where the organic solvent, which is added in slight excess to maintain quality (dispersibility), has seeped out to the surface.
[Causes and Supplementary Notes]
- It may occur when subjected to excessive shock or vibration.
- It is known to occur more easily when transported after being left in high-temperature conditions, or when the product has been subdivided.
- This phenomenon does not mean that the performance as ALPASTE® has deteriorated, so please stir well until the entire contents of the can are uniform before use. There is no problem with the quality.
Regarding fatty acid precipitation
In the case of Leafing ALPASTE®, the fatty acid precipitation phenomenon refers to a state where fatty acids, which are added in slightly larger amounts to maintain quality (leafing stability in the paint), precipitate as a white substance on the surface.
This occurs when the product is stored at low temperatures, as the dissolving power of the blended solvent decreases, causing the fatty acids that can no longer be dissolved to precipitate on the surface.
[Causes and Supplementary Notes]
- It is known to occur more easily when temperatures are low in winter.
You can use it without any issues by stirring it thoroughly as is, or by warming it (to about 30°C) to redissolve it before use.
In winter, please also be aware that the dissolving power of the solvent itself in the paint may decrease, so please take this into consideration. - ALPASTE®, which is formulated with a solvent that has high dissolving power for fatty acids, can also be provided upon request.
This product can mitigate fatty acid precipitation. However, please note that you must be careful regarding its suitability as a paint.
Regarding poor dispersion
Poor dispersion can occur due to factors mentioned in the transportation, handling, and storage sections, such as damage to the container or an improperly sealed can lid, which leads to the evaporation of organic solvents or the ingress of rainwater or foreign matter.
[Causes and Supplementary Notes]
- If the container has been opened and some of the contents removed, leaving a large empty space inside, it is preferable to use the product as quickly as possible, especially for products containing volatile solvents like processed goods.
However, if it is only a minor dispersion failure, it can be resolved to some extent using a high-speed rotating stirrer.

ALPASTE®" width="100%" height="auto" />